Spectroscopic Ellipsometry for the In-situ Investigation of Atomic Layer Depositions
About this book
Project Report from the year 2014 in the subject Chemistry - Other, grade: 1.0, Dresden Technical University (Technische Universität Dresden), course: Semiconductor Technology, language: English, abstract: Atomic Layer Deposition (ALD) is a special type of Chemical Vapor Deposition (CVD) technique based on self-terminating sequential gas reactions for a conformal and precise growth down to few nanometers range. Ideally due to the self-terminating reactions, ALD is a surface-controlled process, where process parameters other than the
choice of precursors, substrates, and deposition temperature have little or no influence. In spite of the numerous applications of growth by ALD, many chemical and physical processes that control ALD growth are not yet sufficiently
understood.
Aim of this student research project is to develop an Aluminium Oxide (Al 2 O 3 ) ALD process from trimethylaluminum (TMA) and Ozone in comparison of two shower head designs. Then studying the detailed characteristics of Al 2 O 3 ALD process using various measurement techniques such as Spectroscopic Ellipsometry (SE), x-ray photoelec-
tron spectroscopy (XPS), atomic force microscopy (AFM). The real-time ALD growth was studied by in-situ SE. In-situ SE is very promising technique that allows the time-continuous as well as time-discrete measurement of the actual growth over an ALD process time. The following ALD process parameters were varied and their inter-dependencies were studied in detail: exposure times of precursor and co-reactant as well as Argon purge times, the deposition temperature, total process pressure, flow dynamics of two different shower head designs. The effect of varying these ALD process parameters was studied by looking upon ALD cycle attributes. Various ALD cycle attributes are: TMA molecule adsorption (M ads ), Ligand removal (L rem ), growth kinetics (K O3 ) and growth per cycle (GPC).
Information
Table of contents
- Contents
- Lists of Abbreviations and Symbols
- Lists of Figures and Tables
- Introduction
- I Theoretical Part
- II Experimental Part
- III Appendix
Trusted by 375,005 students
Access to over 1.5 million titles for a fair monthly price.
Study more efficiently using our study tools.
Frequently asked questions
Yes, you can cancel anytime from the Subscription tab in your account settings on the Perlego website. Your subscription will stay active until the end of your current billing period. Learn how to cancel your subscription
No, books cannot be downloaded as external files, such as PDFs, for use outside of Perlego. However, you can download books within the Perlego app for offline reading on mobile or tablet. Learn how to download books offline
Perlego offers two plans: Essential and Complete
- Essential is ideal for learners and professionals who enjoy exploring a wide range of subjects. Access the Essential Library with 800,000+ trusted titles and best-sellers across business, personal growth, and the humanities. Includes unlimited reading time and Standard Read Aloud voice.
- Complete: Perfect for advanced learners and researchers needing full, unrestricted access. Unlock 1.5M+ books across hundreds of subjects, including academic and specialized titles. The Complete Plan also includes advanced features like Premium Read Aloud and Research Assistant.
We are an online textbook subscription service, where you can get access to an entire online library for less than the price of a single book per month. With over 1.5 million books across 990+ topics, we’ve got you covered! Learn about our mission
Look out for the read-aloud symbol on your next book to see if you can listen to it. The read-aloud tool reads text aloud for you, highlighting the text as it is being read. You can pause it, speed it up and slow it down. Learn more about Read Aloud
Yes! You can use the Perlego app on both iOS and Android devices to read anytime, anywhere — even offline. Perfect for commutes or when you’re on the go.
Please note we cannot support devices running on iOS 13 and Android 7 or earlier. Learn more about using the app
Please note we cannot support devices running on iOS 13 and Android 7 or earlier. Learn more about using the app
Yes, you can access Spectroscopic Ellipsometry for the In-situ Investigation of Atomic Layer Depositions by Varun Sharma in PDF and/or ePUB format, as well as other popular books in Physical Sciences & Chemistry. We have over 1.5 million books available in our catalogue for you to explore.